Bidirectional Self-Folding with Atomic Layer Deposition Nanofilms for Microscale Origami

Baris Bircan, Marc Z. Miskin, Robert J. Lang, Michael C. Cao, Kyle J. Dorsey, Muhammad G. Salim, Wei Wang, David A. Muller, Paul L. McEuen, and Itai Cohen
Jun, 2020

Nano Letters 20, no. 7 (2020): 4850-4856.